During the injection process, the level of molten steel will gradually decrease. When it reaches a critical value, vortices will appear in the upper area of the threading hole and pull the slag into the bucket. When the ball limiting the slag is placed in the curls, the ball The molten steel will flow out of the gaps between the confining balls and the drain holes to reduce the total amount of flowable slag.
KS series of slag limiting balls have been developed and patented by KINGSTONE. They have outstanding characteristics of high strength, high accuracy of casting and efficiency of slag management.
Brand |
KS-SLB-10 |
|
Chemical Composition(%),≥ |
SiO2 |
10 |
Fe2O3 |
40 |
|
Al2O3 |
12 |
|
Bulk Densty(g/cm³),≥ |
110℃*24h |
4.0 |
Modulus of Rupture(MPa) ≥ |
110℃*24h |
6 |
Cold Crushing Strengh(MPa), ≥ |
110℃*24h |
40 |